I have not done much lately, but as I was cleaning up some of the parts, I noticed that the motor seal didn't look quite right. I like to use a 6mm wide double lip seal, but I have used a 5mm single lip seal when I couldn't find the other. I guess all the builder had was an 8mm seal. These are way too wide and bind up the motor against the motor pulley and case. His solution? Get out the belt sander!!!. Now, this might work, but I don't think for long, as the lip holding the spring in is almost non-existant.
I have sent the cylinder to Wayne, as he thinks he can have it Tig welded and then resleeved. The wall thickness on a 150cc cylinder is very thin, and I am going to have it resleeved back to a 125cc overbore size.